The bowl on top of the canopy holds the gas and spreads it over the silica mat. You can buy something and cut it down, or have one made. Either way it needs a good gas fitting, which is covered in full below.

What we'd do

  1. Buy the stainless pot for the first test. It's cheap and quick, and shows you how the fire behaves.
  2. If the design stays, have a stainless drum made with the top plate job. It has a thicker top for the fitting and a properly flat base.
  3. Avoid galvanised steel and aluminium. Galvanised gives off zinc fumes and aluminium softens in the heat.

Buy or make: every option

OptionRouteCostSizeWeldingGood and bad
Stainless pot, cut down Buy฿300–700Ø300 × 130TIG, thin wallFlat top takes the fitting well. The cut edge needs flattening. Single-layer base only.
Stainless wok Buy฿965Ø320 × 95TIG, thin wallLow, smooth shape, and the top is curved so the fitting needs care. Uncoated only.
Stainless mixing bowl Buy฿339Ø320 × 110TIG, very thinCheapest. Very thin, so it needs a reinforcing pad and it may burn through.
Carbon-steel wok Buy฿399Ø320 × 95Any welderEasy to weld, same metal as a steel canopy. It rusts, so needs 600 °C paint.
Stainless drumMakeabout ฿1,500–3,500 (estimate)Ø300 × 130Shop TIGBest long-term choice: any height, thick top, flat flange. Costs more and needs a shop.
Mild steel drumMakeabout ฿800–2,000 (estimate)Ø300 × 130Any welderSame shape in cheaper metal that any workshop can weld. Scales and rusts faster.
Five-sided steel hoodMakequoteØ300+ × 120Any welderMatches the canopy's shape. Most welding and more seams to leak-test.
Spun or pressed domeMakequote, likely highanyShop TIGBeautiful and smooth, but needs a metal spinner and may be slow to arrange.

Prices for made items are rough estimates until a shop quotes them. Choose or change the bowl in the Planner, under "Bowl on top".

Buying a pot or wok

  • Check it is really 304. Cheap "stainless" may be 201, which handles heat and corrosion worse. Ask for the grade, and test with a magnet: 304 should barely stick, though forming can make it slightly magnetic.
  • Single-layer base. A thick "sandwich" base has aluminium inside, so it can't be welded properly.
  • No coating. Non-stick or honeycomb coatings burn off and give off fumes.
  • Measure the wall. Thin pots are often 0.6–1 mm. Under about 1.2 mm, weld the fitting to a pad (option 2 below).
  • Size: it must cover the 280 mm hole, with its wall clear of the holder rods on the Ø360 circle.

Cutting it down

  1. Take off handles and rivets, then fill any holes they leave.
  2. Mark the height all the way round with tape, about 130 mm from the pot's base.
  3. Cut with a thin stainless cutting disc. Use a stainless-only disc so it won't contaminate the metal.
  4. Rub the cut edge flat on sandpaper laid on a steel plate. It has to sit flat on the top plate all the way round.
  5. Clean off grease before welding, as leftover oil can cause porous welds.

Making a bowl from steel

PartSizeMaterialWeight
Top discØ300 × 2 mm304 stainless, or mild steel1.1 kg
Wall, rolled and seam-weldedabout 945 × 130 × 1.5 mmSame1.5 kg
Base flangeOD 330, ID 280, 3 mmSame0.6 kg
Gas fitting3/8" half couplingSame metal as the top—
  1. Laser-cut the disc and flange, with the top plate job so they all ship together.
  2. Roll the wall to Ø300 and weld the seam fully.
  3. Weld the wall to the disc and to the flange, inside or outside, with a full gas-tight seam.
  4. Cut the 12 mm hole and weld on the fitting (see below).
  5. Test the weld before fitting. The safest check is a dye-penetrant kit on the weld. If you air-test instead, clamp the pot's open base to a board with a gasket and use no more than about 0.5 psi (35 mbar), through a low-pressure regulator, standing clear. Then brush the seams with soapy water. Higher pressure can throw the board off: 5 psi pushes on it with about 200 kg of force.

Flange OD 330 keeps it clear of the mat holder's M8 nuts on the Ø360 circle. Mild steel and 304 don't mix with ordinary rods, so weld each pair with suitable filler.

The gas fitting, step by step

This is the joint between the copper gas pipe and the pot, drawn much larger than life.

Fitting options

#FittingUse it whenGood and bad
1Stainless half coupling, 3/8" BSP, TIG-welded over the hole Stainless pot, wall about 1.2 mm or thickerStrong, cheap and heat-proof. You cut a whole coupling in half, and need a TIG welder.
2Same coupling on a stainless pad, Ø50 × 3 mmThin stainless pot, wok or bowlThe pad spreads the load and stops burn-through. Weld the pad to the pot first, then the coupling to the pad.
3Plain steel half coupling or weld socket Carbon-steel wok, mild steel drum or hoodAny welder can do it. Must be black steel, not zinc plated. Paint with 600 °C paint.
4Bolt-through (bulkhead) fitting with a copper or graphite washer each sideNo welder available, or a quick testNo heat needed. It relies on washers, and thin metal can flex, so leak-test often.
5Silver-brazed brass fittingOnly if a skilled brazer recommends itNo melted stainless, but needs the right flux. Joint and brass both have lower heat limits.

Welding the coupling

  1. Cut the coupling in half and clean up the cut end. That end goes down on the pot.
  2. Drill or punch a 12 mm hole in the centre of the pot top and remove the burr.
  3. Screw in a sacrificial steel plug to protect the threads. Don't use a brass or zinc-plated one.
  4. Tack in four places, then run short, cool passes all the way round.
  5. Remove the plug. Run a 3/8" BSP tap through the thread if welding has distorted it.
  6. Screw in the brass adaptor with LPG-rated thread sealant. Fit the copper with its flare nut.
  7. Pressure up and leak-test with soapy water.

Details that matter

  • Why not galvanised? Welding or heating zinc gives off toxic fumes, and the coating burns away. If only galvanised is available, choose a different fitting.
  • Thread types: 3/8" BSP has a 16.7 mm outer diameter and 19 threads per inch. Check whether the coupling is parallel or tapered and match the adaptor to it.
  • Flare side: 3/8" flare on the copper, with no tape or sealant on the flare cone. Metal seals against metal.
  • Support the pipe. Clip the copper within 300 mm of the bowl so its weight can't lever the thin top or crack the weld.
  • Check the temperature. On the first burn, measure the fitting with a contact thermometer. Brass and sealants have limits, and if it gets near the sealant's rating, change to a suitable high-temperature one or move the joint.
  • Spreading the gas: if the middle of the mat burns harder than the edge, weld a small Ø80 baffle disc under the fitting on three short legs. Test first, as it may not be needed.